RELANETRELANET

Automotive Interior Adhesive Manufacturer · Guangzhou, China

Automotive Interior Adhesives Proven on Nissan, Honda and BYD Production Lines

Waterborne PU, APAO and PUR hot melt, and light-transmitting adhesive film for door panels, instrument panels, seats, trunk trim and illuminated parts. We tune each formulation to your substrate, climate and cycle time, then help your part through OEM validation to SOP.

Standard samples ship in about 3 days · An engineer replies within 1 working day

Car interior console with an illuminated ambient lighting strip along the trim
  • IATF 16949

    Certificate IATF/T19001-2026

  • ISO 9001 · 14001 · 45001

    Quality, environment, health & safety

  • 4 automotive groups · 10+ vehicle programs

    Nissan, Honda, BYD, Toyota

  • ~960 t / year

    Production capacity with headroom for new programs

  • 2 g/L VOC

    R-5670, SGS-tested to GB 33372 (limit 50 g/L)

“We can’t afford another adhesive that fails at the OEM approval stage.”

You have a nomination date, a new skin, and an adhesive that keeps failing odor or peel tests. Here is what we fix:

  • The adhesive passes the lab but fails the OEM’s odor or VOC test, and months of work are lost.

    We screen emissions at the selection stage. R-5670 measured 2 g/L VOC (SGS, GB 33372) and odor intensity 2.3 by the Nissan VES method, with formaldehyde, benzene series and TVOC not detected.

  • Peel strength drops on a new skin, and everyone blames the glue.

    Our engineers test skin, substrate, process and environment separately. On one Nissan program, peel was 5–10 N against a 19 N target. We traced it to the skin’s knit fabric, and the customer fixed it with a nonwoven layer.

  • Backlit trim yellows, bubbles or shows moiré, and OCA can’t handle a curved, high-stress part.

    RY-10 light-transmitting film: >99% transmittance, ΔE ≈ 1.0 after 110°C × 1,500 h, and IR activation with 35 s pressing. No vacuum de-bubbling.

  • Slow initial tack holds up the press, so parts wait and cycle time suffers.

    R-5670 reaches about 25 N/25 mm peel 1 minute after lamination, and about 60 N/25 mm after 7 days.

  • Imported suppliers won’t adjust a formula for one line, and their answers take weeks.

    We adjust open time, activation temperature, solids, tack balance, color and heat limit. Custom samples are ready in 7 working days.

  • Your solvent line must go waterborne, but PP pretreatment and drying are new to the team.

    We map the conversion step by step: flame treatment, a 4-hour wrapping window, oven drying and wrapping order. Then we tune the line with you.

“Why pay attention to a material that is a tiny share of the part cost?”

Because the adhesive is cheap, and a failure is not. The adhesive on a door panel costs roughly RMB 5–8. Reworking a delaminated part can exceed RMB 800 per vehicle, about 100 times more.*

That is why we price on total cost, not on price per kilogram:

  • Coat weight

    What changes with RELANET
    Waterborne PU at ~47–50% solids. A kilogram of waterborne adhesive carries roughly 500 g of solids, compared with about 100 g for solvent-based contact cement.*
  • Pretreatment

    What changes with RELANET
    R-7110 APAO bonds qualified clean PP without primer, flame or plasma treatment.
  • Spray vs. film

    What changes with RELANET
    In an industry cost example, pre-formed adhesive film came to RMB 12.5/m² against RMB 14.8/m² for spraying once labor, exhaust treatment and waste were counted.*
  • Price

    What changes with RELANET
    Typically below imported brands, with tiered pricing by annual volume.

*Industry estimates from our project experience. We replace them with numbers from your own project during the assessment.

Automotive Interior Adhesives: Five Technologies, One Engineering Team

Each grade has a series-production record or validation data. Pick by substrate, process and durability target.

  • Wrapped automotive door panel bonded with two-component waterborne PU adhesive

    2K Waterborne PU (PUD)

    RELANET R-5670 + R-60C

    Best for
    Instrument panels, door panels, seats, armrests, trunk trim
    Proof
    Nissan N7 / N6 / NX7, BYD Denza Z9GT, GAC Toyota Camry
  • Glowing light paths representing light-transmitting adhesive film for backlit trim

    Light-Transmitting Adhesives

    RY-10 film, R-60 film, R-5610 waterborne

    Best for
    Backlit trim, ambient lighting panels, illuminated logos
    Proof
    Honda Ye P7 / Ye S7, GAC Toyota V57
  • Automotive interior parts production line using APAO hot melt adhesive

    APAO Hot Melt

    R-7110, R-7206

    Best for
    Door inserts, spare wheel covers, sunroof frames, harness fixing
    Proof
    Nissan Sylphy, GAC Honda Ye P7
  • Acoustic foam texture of the kind laminated with waterborne chloroprene adhesive

    Waterborne Chloroprene

    R-5110

    Best for
    Foam, felt, acoustic and NVH parts
    Proof
    FAW Toyota Corolla
  • Leather car seat skin of the kind laminated with reactive PUR hot melt

    Reactive PUR Hot Melt

    R-9610, R-9655, R-9692

    Best for
    Deep-draw wrapping, leather and microfiber skins, roll lamination
    Proof
    R-9610 main production grade; BYD spare wheel cover program planned · R-9655 / R-9692 new

Find the Adhesive by Interior Part

Most interior bonding problems are part-specific. Start with your part.

  • Car cabin at night with illuminated interior trim and ambient lighting

    Illuminated interior trim

    Ambient lighting panels, hidden-till-lit logos, smart surfaces. Bonding layers that stay clear, flat and bubble-free.

    Illuminated trim solutions
  • Close-up of a wrapped door panel insert and handle trim

    Door panels, instrument panels, armrests and pillars

    Deep draws, folded edges and tight radii, by hand wrapping or vacuum forming.

    Door & instrument panels
  • Car trunk with carpeted trunk trim and spare wheel cover

    Trunk trim, spare wheel covers and reinforcements

    Flocked fabric on PP or paper honeycomb, plus robotic hot melt for sunroof frames.

    Trunk trim & reinforcements
  • Car interior showing the headliner, seats and trim surfaces

    Headliners, seats and acoustic parts

    Large-area spraying, foam and felt lamination.

    Headliners, seats & NVH parts

Matched to Your Lamination Process, Not the Other Way Around

There is no best process. There is only the process that fits your part, your material and your volume. We qualify adhesives for six wrapping routes, and we start where 90% of debonding starts: the substrate interface.

  • Hand wrapping

    What usually goes wrong
    Short open time, cracking on cold winter mornings
    Our recommendation
    R-5670 hand-wrapping version, open time 8–15 min
  • Hot press

    What usually goes wrong
    Mold gaps, poor IR activation, blisters from hot demolding
    Our recommendation
    High-tack R-5670
  • Silicone membrane vacuum press

    What usually goes wrong
    No way to measure or cool the bond line
    Our recommendation
    R-5670, where initial tack does the holding
  • Hot melt roll coating

    What usually goes wrong
    Equipment cleaning, wrinkles on stretched skins
    Our recommendation
    R-7110 / R-7206 APAO, R-9610 PUR
  • Pre-coated adhesive film

    What usually goes wrong
    Four parties must align on one bond line
    Our recommendation
    RY-10 film
  • Robotic spraying and dispensing

    What usually goes wrong
    Hand know-how does not transfer to robots
    Our recommendation
    R-5670 with IR re-activation, R-7206

Low VOC, Low Odor and Long-Term Durability, With the Numbers

Buyers ask us for numbers, not adjectives. Here are some from third-party reports and our own test records:

  • VOC content, R-5670

    2 g/L

    limit 50

    GB 33372-2020, SGS

  • Odor intensity, R-5670

    2.3

    irritation 0

    Nissan VES M00-08, 90°C × 4 h, SGS

  • Aldehydes, benzene series, TVOC

    Not detected

    Nissan VES M00-03 / M00-12, SGS

  • Odor, PUR hot melt

    2.5–3.0

    entry limit ≤3.5

    VDA 270

  • VOC, PUR hot melt

    41.6 mg/kg

    entry limit ≤50

    VDA 278

  • Fogging, PUR hot melt

    0.32 mg

    entry limit ≤0.5

    DIN 75201

  • Anti-yellowing, RY-10

    ΔE ≈ 1.0

    110°C × 1,500 h

  • Humidity aging, waterborne PU

    85% peel retention

    60°C / 95% RH × 1,000 h

Typical values on tested specimens. Validate on your own substrate, process and OEM standard.

Two Problems We Are Asked to Solve Most

  1. 1

    Moving from solvent to waterborne adhesive

    OEM emission targets are pushing solvent contact cement out of interior plants. The switch adds two steps: PP pretreatment and oven drying. We provide the conversion checklist, tune the drying and activation window, and support the first parts on your line.

    Plan your solvent-to-waterborne conversion
  2. 2

    Blisters, edge lifting, odor failures and winter bonding

    In our projects, fewer than 5% of bonding failures turn out to be caused by the adhesive itself. Most begin at the interface or in the process: mold gaps, expired surface treatment, wrong mixing ratio, cold storage. Our troubleshooting guide walks through each symptom.

    Open the troubleshooting guide

Production-Proven on These Vehicle Programs

  • Dongfeng Nissan

    Vehicle program
    N7 · N6 · NX7
    RELANET grade
    R-5670
  • Dongfeng Nissan

    Vehicle program
    Sylphy
    RELANET grade
    R-7110
  • GAC Honda

    Vehicle program
    Ye P7
    RELANET grade
    R-7206 · RY-10
  • Dongfeng Honda

    Vehicle program
    Ye S7
    RELANET grade
    RY-10
  • BYD / Denza

    Vehicle program
    Z9GT spare wheel cover
    RELANET grade
    R-5670
  • GAC Toyota

    Vehicle program
    Camry door panel · Bozhi 3X
    RELANET grade
    R-5670
  • GAC Toyota

    Vehicle program
    V57
    RELANET grade
    R-5610
  • FAW Toyota

    Vehicle program
    Corolla acoustic parts
    RELANET grade
    R-5110

Featured cases

  • Illuminated trim for Honda Ye P7 and Ye S7

    From a 2022 development start to Honda approval in 2024 and series production.

    Read the case
  • EV door panels for Nissan N7 programs

    A solvent-to-waterborne switch and a peel problem traced to the skin.

    Read the case
  • Spare wheel cover for BYD Denza Z9GT

    Flocked fabric on PP and paper honeycomb. Every test ended in substrate failure, not adhesive failure.

    Read the case

Not Sure Which Technology Fits? Compare Before You Sample

  • Waterborne PU vs. PUR vs. APAO vs. solvent

    A decision tree by station temperature, cycle time, substrate, emission target and equipment. PUR needs sealed equipment; APAO does not.

    Compare adhesive technologies
  • Light-transmitting film vs. OCA and double-sided tape

    OCA is designed for flat, rigid-to-rigid bonding. Backlit trim is rigid-to-soft, curved and highly stressed.

    Compare film vs. OCA
  • Replacing an imported grade?

    Send us the grade you use today, such as a TECHNOMELT®, AQUENCE®, SikaMelt® or SikaTherm® product. We’ll run a side-by-side test on your substrate, free of charge.

    Imported grade alternatives

Trademarks belong to their respective owners. RELANET is not affiliated with them.

Supplying Interior Plants Across the World

We ship direct from Guangzhou with English TDS and SDS, a website in your language, and remote video support. We are building a network of local partners. Many of our customers are Chinese Tier 1 suppliers following automakers into new plants. Others are local interior suppliers looking for a responsive second source.

  • North America

    Low-VOC data, FMVSS 302 flammability tested, competitive landed cost

  • Mexico

    Experience with Nissan and Honda standards, a Spanish-language website

  • Brazil & South America

    Humidity-resistant formulations for hot, humid plants

  • Southeast Asia

    Support for solvent-to-waterborne switching in humid climates

  • Europe

    VDA 270 / 278 and DIN 75201 data, REACH and ELV declarations

  • Japan & Korea

    Series production to Japanese OEM standards

  • Russia & Central Asia

    Cold-climate grades and winter-safe shipping

  • China

    Engineers on site within 24 h in South China and 48 h in East, North and Central China

From Material Data to SOP: Eight Steps We Run With You

“We don’t just sell adhesive. We help you take a wrapped part through validation to series production.”

  1. 01

    Define material inputs.

    You share substrate, skin and process; we review them.

  2. 02

    Supply trial materials.

    You send 1–2 m² of skin and substrate for flat-panel screening.

  3. 03

    Issue test findings.

    We report feasibility before you invest in tooling changes.

  4. 04

    Trial on real parts.

    We test together on your parts and equipment.

  5. 05

    Record process parameters.

    We log dimensions, coat weight, temperature and cycle time.

  6. 06

    Compile part-level results.

    We prepare data you can submit to the OEM.

  7. 07

    Finalize work instructions.

    If the result is OK, we issue the process specification. If not, we revise and repeat.

  8. 08

    Implement SOP.

    We support the launch and follow up in production.

Free technical services

Samples, side-by-side tests, pre-validation testing to NES M0160 (Nissan), 0095Z-SDA (Honda) and BYD interior standards, on-site process tuning, and failure analysis.

Custom Formulation

Open time, activation temperature, solids, initial and final tack, curing-agent color (blue for visual coat-weight control, clear for light-colored parts) and heat limit can all be tuned. Custom samples in 7 working days; lab development in 1–2 months. NDA available.

Start a custom formulation

OEM & Private Label Supply

Building your own adhesive line for automotive interiors? We produce RELANET-qualified formulations under your brand:

  • Your label and your product name, with technical documents prepared to your format
  • Formulation and your process know-how kept confidential under NDA
  • The same batch testing, retained samples and change control as our own grades
Discuss OEM / private label supply

Packaging Built Around Your Line

Packaging sizes can be customized to your consumption and handling. Our standard formats include 20 kg pails for PUR hot melt and adhesive film rolls from 1 roll (100 m²), with film thickness of 40–200 μm and die-cut shapes on request. Waterborne adhesives ship with frost protection (kept above 5°C), and PUR is sealed against moisture.

Delivery You Can Plan Around

Standard samples
About 3 days to ship, free (about 5 kg)
Custom samples
7 working days
Standard orders
7–10 days
Rush orders
About 3 days
MOQ
Small batches accepted; no MOQ during new-program ramp-up
Capacity
About 960 tonnes per year, with headroom for new programs
Overseas
Direct from Guangzhou; 30% deposit, balance before shipment

Your Concerns, Answered

  • “Will it pass my OEM’s approval?”

    How we address it
    Pre-validation testing to the OEM standard before your submission
    Proof
    Series production with Nissan, Honda, BYD and Toyota programs
  • “Is the quality consistent batch to batch?”

    How we address it
    Incoming material checks, in-process control, batch testing, retained samples
    Proof
    IATF 16949 (IATF/T19001-2026); viscosity variation ≤3% between batches
  • “What if the formula changes without notice?”

    How we address it
    Formal change control under IATF 16949; PCN supported
    Proof
    Change records kept in our system
  • “Is a small supplier safe for a long program?”

    How we address it
    Capacity headroom, price lock during framework agreements
    Proof
    About 960 t/year capacity
  • “Who pays if the adhesive is at fault?”

    How we address it
    Compensation terms written into the contract
    Proof
    Claims honored in past projects
  • “Can I test with a small quantity first?”

    How we address it
    Free samples; small batches; no MOQ during ramp-up
    Proof
    Film from 1 roll (100 m²)
  • “Will my process know-how stay private?”

    How we address it
    NDA available; your process is never shared
    Proof
    Signed with strategic customers
  • “Can I see the factory?”

    How we address it
    Supplier audits welcome; book a visit
    Proof
    Audits hosted every year; Huangpu, Guangzhou

A Focused Adhesive Maker, Not a Trading Company

RELANET was founded in August 2021 in Huangpu, Guangzhou, to develop adhesives for automotive interior and exterior trim. About 60% of our team works in R&D. Our core team has spent years in automotive interior bonding, and our engineers deal directly with your process and quality teams.

  1. 2022

    Started development of illuminated-trim bonding

  2. 2024

    Light-transmitting bonding system approved by Honda; Ye P7 and Ye S7 enter series production

  3. 2025

    Waterborne PU adhesive launched on Dongfeng Nissan N7

  4. 2026

    R-5610 light-transmitting waterborne adhesive passes GAC R&D Center testing; R-5670 approved by BYD for trunk trim

Adhesive laboratory where engineers test interior bonding formulations

Our working principles

  • Rigorous

    110°C humidity aging, 1,500 h anti-yellowing

  • Innovative

    Hard-to-bond substrates and light-transmitting parts

  • Reliable

    OEM series-production approval

  • Sustainable

    Waterborne and hot melt chemistry with low VOC

Engineering Notes for Interior Bonding Teams

  • How to Bond Backlit Interior Parts Without Bubbles

    Why vacuum de-bubbling isn’t the only option for illuminated trim.

  • How to Convert a Solvent Adhesive Line to Waterborne PU

    The two new steps and the four details most teams miss.

  • VDA 270 Odor Test Explained for Interior Adhesives

    What the grades mean and where adhesives fail.

Questions Buyers Ask Before Their First Inquiry

  • Are samples free, and how fast do they ship?

    Yes. Standard samples (about 5 kg) are free and ship in about 3 days. Custom samples take 7 working days.

  • What is your MOQ?

    We accept small batches, and there is no MOQ during a new program’s ramp-up. Adhesive film starts from 1 roll (100 m²).

  • What are your lead times?

    Standard orders ship in 7–10 days, and rush orders in about 3 days.

  • Do you offer OEM or private label supply?

    Yes. We can supply under your brand with your labels and documents, and we keep your formulation and process confidential under NDA.

  • Can packaging be customized?

    Yes. Pack sizes can be adapted to your consumption and handling. Film rolls are available in thicknesses from 40 to 200 μm, and die-cut shapes are available.

  • Are you IATF 16949 certified?

    Yes, certificate IATF/T19001-2026. We also hold ISO 9001, ISO 14001 and ISO 45001.

  • Do you charge for technical support?

    No. Samples, side-by-side tests, pre-validation testing and on-site process tuning are free.

  • How do overseas orders work?

    We ship direct from Guangzhou with English TDS and SDS. Payment is a 30% deposit with the balance before shipment.

Tell Us Your Part. We’ll Recommend a Grade and Ship Samples.

Share your substrate, skin, part, process and target cycle time. An engineer replies within 1 working day.

Quick inquiry form

* Required

Or reach us directly

  • WhatsApp

    +86 159 1457 0351

    Chat now
  • WeChat

    Scan the QR code

    QR code coming soon